WebHeat treating 80CrV2: heat to 830 C (1525 F) hold for 10 mins for "knife blade thickness" Quench in a fast quench oil (not Canola) Temper immediately at 204 C (400 F) for 2 … WebJul 20, 2016 · Another issue with 80CrV2 is that it comes heavily spheroidized (or, at least much of what has reached the knifemakers' market lately does), so in order to get good results you have to normalize and … do grades motivate students to succeed in school Web80CrV2 Carbon Steel Information and Composition. Condition: This alloy been properly annealed and is in the soft condition. You do not have to do any non-standard wasteful processes before heat treating. The steel … do grades really matter in college reddit WebSep 6, 2024 · It was a preferred choice for beginner knife makers due to its simple heat treatment. 8670 Steel Composition. Carbon C 0.75%: Increases the edge retention, hardness and tensile strength. It also improves steel resistance to wear, abrasion and corrosion. ... 8670 vs 80CrV2. These two steels are very similar in properties and offer … WebFeb 27, 2024 · Normalize 1600/1530/1475/1300 (optional). The sub critical cycle is to add toughness. A soak (or holding time) is recommended but not necessary. 2 minutes is … do grades really matter essay WebNov 23, 2024 · These two steels, 52100 and 80CrV2, are not at all similar and should not even be in the same sentence when discussing a heat treating regimen. Industry …

Post Opinion